Answer
High chloride levels aggressively attack stainless steel, leading to stress corrosion cracking, especially in high-temperature environments like boilers and condensers. Monitoring cycles of concentration is vital. Operators use the Chloride Test Kit to determine the exact moment a system requires blowdown or dilution.